Einführung

Selecting the right colorant for engineering plastics is a complex process. While many organic pigments, inorganic pigments, and solvent dyes work well for general thermoplastics, high-performance materials like Nylon (Polyamide) have strict requirements.

Below, we explore the five critical performance characteristics colorants must possess for successful Nylon injection molding[^1].

1. Heat Resistance and Lightfastness

The processing temperature of the resin dictates the stability requirements for the colorant. As shown in the table below, Polyamide (Nylon) requires some of the highest processing temperatures among engineering plastics[^2].

Processing Temperatures and Colorant Requirements by Resin Type

Resin TypeProcessing Temp (℃)Key Colorant Requirements
Polyamid (Nylon)270 - 290Heat resistance, Water-free, Good dispersion
Polyester270 - 290Heat resistance, Non-migrating, Neutral pH
ABS230 - 310Heat resistance, Good dispersion
Polypropylene230 - 280Heat resistance, Good dispersion
Polyurethane210 - 270Lightfastness, Acid/Reduction resistance
PMMA200 - 230Fastness, Heat resistance, Non-migrating
PVC180 - 250Good dispersion, Acid resistance
Polystyrene180 - 240Fastness, Good solubility
Polycarbonat150 - 200Heat resistance, Water-free, Good dispersion
HDPE160 - 230High thermal stability, Non-migrating
LDPE150 - 220Excellent fastness, Non-migrating

> Anmerkung: Due to the high processing temperatures of Polyamide, colorants must exhibit exceptional thermal stability. Many organic pigments can negatively affect the properties of the Nylon melt, limiting the selection to specific high-performance pigments with good lightfastness.

Molten nylon plastic during high temperature injection molding process.

2. Chemical Stability

There must be no chemical reaction between the colorant and the resin, nor should the colorant promote resin decomposition.

Polyamide resins (PA) are highly active. In their molten state, they exhibit reducing properties, which can easily cause colorants to shift in hue or degrade. Therefore, the choice of colorants for Nylon is limited to those with high chemical inertness.

3. Migration Resistance

Migration refers to the movement of the colorant within the polymer or to the surface. There are three main types:

  • Solvent Extraction: Leaching of color in water or organic solvents.
  • Contact Migration: Staining of adjacent objects or packaging.
  • Blooming (Surface Frosting): The colorant has high solubility at high heat but low solubility at room temperature, causing it to migrate to the surface as the part cools.

Inorganic vs. Organic: Generally, inorganic pigments are heterogeneously dispersed in polymers and rarely bloom. In contrast, organic pigments have varying degrees of solubility in polymers, making them more prone to migration issues.

Comparison of plastic part surface quality showing pigment blooming.

4. Tinting Strength

Tinting strength determines the dosage of colorant required to achieve the target color.

  • Particle Size: Generally, tinting strength increases as the pigment particle size decreases.
  • Organic vs. Inorganic: Organic pigments[^3] typically have higher tinting strength than inorganic pigments.
  • Mixing: Tinting strength can be significantly improved when colored pigments are used in combination with white pigments.

5. Dispersion

For optimal coloring results, the colorant must be uniformly dispersed in the polymer as microscopic particles.

Pigments often contain many aggregated particles. To achieve the desired quality, high shear force is required during the compounding process to break down large aggregates into smaller clusters. Poor dispersion leads to color streaks and weak points in the final part.

High shear dispersion of pigments in polymer masterbatch.


[^1]: Explore this resource to gain insights into optimal techniques and tips for successful Nylon injection molding. [^2]: Explore this resource to gain in-depth knowledge about engineering plastics, their properties, and applications in various industries. [^3]: Organic pigments can offer vibrant colors and higher tinting strength, making them valuable for specific applications.

Über den Autor

Alex Yu

Alex Yu

Ideal Pro Manufacturing

Alex ist Mitbegründer von Ideal Pro, doch wenn er nicht gerade wichtige Projekte beaufsichtigt oder das technische Team leitet, trifft man ihn wahrscheinlich auf einer langen Radtour, auf der Suche nach dem besten Kaffee der Stadt oder bei der Planung seines nächsten Reiseabenteuers. Mit über 20 Jahren Erfahrung in den Bereichen internationaler Vertrieb und Projektmanagement hat er schon alles gesehen – enge Fristen, knifflige technische Probleme und alles, was dazwischen liegt. Er ist davon überzeugt, dass großartige Arbeit von einem ausgeruhten Geist und einer guten Tasse Kaffee entsteht, und er bringt dieselbe Neugier und Liebe zum Detail in jedes Projekt ein, das er übernimmt. Wenn er nicht im Büro ist, befindet er sich meist irgendwo im Freien, erkundet neue Orte und sammelt Geschichten, die er gerne weitergibt.

Aktuelle Blog-Beiträge

Polycarbonat-Spritzgießen: Feuchte, Spannung und der Preis der Klarheit
Spritzguss

Polycarbonat-Spritzgießen: Feuchte, Spannung und der Preis der Klarheit

Feuchtigkeit bewirkt bei Schmelztemperatur eine Hydrolyse von Polycarbonat, sodass ein klares, glänzendes Bauteil dennoch einen Falltest nicht bestehen kann. Der Feuchtigkeitsgrenzwert, die Prüfung auf Restspannungen, die Vergleichszahlen von PC und PMMA sowie die Fälle, in denen PC unabhängig vom Verfahren das falsche Material ist.

Blog-Avatar Alex Yu
19. November 2026
ABS-Spritzgießen: Typwahl, Prozessfenster und wo ABS versagt
Spritzguss

ABS-Spritzgießen: Typwahl, Prozessfenster und wo ABS versagt

Güteklassen mit den sie unterscheidenden Zahlen, das Schmelz- und Formfenster mit den jeweiligen Bruchstellen an den Kanten, die Berechnung der relativen Teilekosten, eine Tabelle zur Fehlerklassifizierung sowie die vier Betriebsbedingungen, die das ABS-Gespräch beenden.

Blog-Avatar Alex Yu
19. November 2026
Schwarzoxidation: was eine ein Mikron dicke Konversionsschicht leistet und nicht leistet
Spritzguss

Schwarzoxidation: was eine ein Mikron dicke Konversionsschicht leistet und nicht leistet

Schwarzoxid ist eine Konversionsbeschichtung, keine Barriere: 0,2 bis 1,5 Mikrometer Magnetit, vernachlässigbare Auswirkungen auf die Passgenauigkeit und ein Korrosionsschutz, dessen Wirksamkeit vollständig von der Zugabe von Öl abhängt. Hochtemperatur-, Mitteltemperatur- oder Raumtemperatur – was soll in die Zeichnung aufgenommen werden, …

Blog-Avatar Alex Yu
19. November 2026
Hochauflösender 3D-Druck: was 25 Mikron nicht über Ihr Bauteil aussagt
3D-Druck

Hochauflösender 3D-Druck: was 25 Mikron nicht über Ihr Bauteil aussagt

Schichthöhe, Mindeststrukturgröße und Maßtoleranz sind drei voneinander unabhängige Grenzwerte. Die Berechnung anhand der veröffentlichten prozessspezifischen Werte, der Aufwand für die Endbearbeitung sowie der Prüfkörper, der dies belegt, bevor Sie das Bauteil freigeben.

Blog-Avatar Alex Yu
18. November 2026