4 Common Injection Molding Defects & Proven Solutions

Alex Yu

Alex Yu

Leestijd: 5 minuten

Publicatiedatum: Jul 10 2026

4 Common Injection Molding Defects & Proven Solutions

Spuitgieten is a highly precise manufacturing process, but it is not immune to production challenges. Whether you are a process engineer or a quality control manager, encountering defects can lead to costly downtime and material waste.

In this comprehensive guide, we break down the four most common injection molding problems—bubbles, sprue sticking, slow production cycles, and short shots—and provide actionable, expert-level solutions to keep your production line running smoothly.

Injection molding machine producing plastic parts on the factory floor.


Bubbles and Voids in Plastic Parts

Bubbles can compromise the structural integrity and aesthetic appeal of a product. They generally fall into two categories: vacuum voids (caused by shrinkage) and gas bubbles (caused by trapped air or moisture). For deeper root cause analysis of internal voids and blisters in thick plastic components, read our dedicated guide: Analyse van bellenvorming bij de productie van kunststofproducten.

Vacuum Voids (Shrinkage)

These typically occur in thick-walled sections where the outer surface cools faster than the core, causing the center to shrink and pull away.

  • Optimize Gate Size: Set the gate height to 50%–60% of the part's wall thickness.
  • Hold Pressure & Time: Ensure adequate packing pressure and extend the holding time slightly beyond the gate freeze-off time to compensate for shrinkage.
  • Adjust Injection Parameters: Lower the injection speed while increasing the injection pressure.
  • Material Selection: Consider using resins with higher melt viscosity for thick-walled parts.

Gas Bubbles

Caused by volatile gases from moisture or material degradation.

  • Pre-Dry the Material: Always follow manufacturer guidelines for drying time and temperature.
  • Control Barrel Temperature: Lower the resin temperature to prevent thermal degradation and gas generation.
  • Improve Flow: If poor flow is causing trapped air, increase both the barrel and mold temperatures, and raise the injection speed.

Close-up of vacuum voids and gas bubbles in an injection molded plastic part.


Sprue Sticking (Main Runner Adhesion)

When the solidified sprue sticks to the mold instead of ejecting with the part, it halts automated production. Here is a quick troubleshooting checklist: Sprue sticking falls under broader ejection and demolding failures; check our full troubleshooting resource: Injection Molding Ejection Problems, Solutions.

Mogelijke oorzaakRecommended Solution
Insufficient Cooling TimeIncrease cooling time to ensure the sprue fully solidifies before ejection.
Inadequate Draft AngleIncrease the draft angle of the main sprue for easier ejection.
Nozzle/Sprue Bushing MismatchCheck the mating dimensions between the nozzle and sprue bushing to prevent flash/leakage.
Poor Surface FinishPolish the sprue channel and ensure a cold slug well is present at the base.
Low Nozzle TemperatureIncrease the nozzle temperature to prevent premature freezing at the tip.

Technical diagram showing proper sprue bushing draft angle and cold slug well design.


Slow Production Cycles

Cycle time directly impacts profitability. If your machine is running slower than expected, consider these optimization strategies: All cycle time improvements rely on properly tuned injection molding process parameters; review our complete parameter tuning guide: Injection Molding Parameters Tuning Guide.

  • Thermal Management: Excessively high plastic or mold temperatures extend cooling time. Optimize cooling channels and reduce temperatures where possible.
  • Plasticizing Efficiency: Reduce back pressure and minimize the use of regrind to prevent material bridging in the hopper. Ensure the feed throat is properly cooled.
  • Machine Kinematics: Optimize hydraulic and servo motor settings to safely increase mold opening/closing and ejection speeds.
  • Mold Design for Automation: Design molds for smooth, automated part ejection to reduce manual intervention.
  • Part Wall Thickness: Excessive wall thickness drastically increases cooling time. Consider core-outs or redesigning the part for uniform, thinner walls.
  • Nozzle Drool: Prevent melt leakage by using a self-locking nozzle or slightly lowering the nozzle temperature.
  • Heater Capacity: If the barrel cannot maintain temperature, upgrade to a machine with higher plasticizing capacity or pre-dry/pre-heat the material.

Infographic showing strategies to reduce injection molding cycle time and increase efficiency.


Short Shots (Incomplete Filling)

Short shots occur when the mold cavity isn't completely filled. This is usually a result of insufficient material, inadequate pressure/speed, or excessive flow resistance.

  • Inadequate Plasticizing: Upgrade to a machine with higher plasticizing capacity and heating power.
  • Component Wear: Inspect the screw, barrel, and check valve for wear that causes material backflow.
  • Heater Failures: Check thermocouples and heater bands; actual barrel temperature may be lower than the setpoint.
  • Hydraulic Leaks: Worn seals in the injection cylinder can cause pressure loss.
  • Nozzle Restrictions: A clogged or misaligned nozzle creates massive pressure drops.
  • Low Mold Temperature: Increase mold temperature to improve melt flow.
  • Unbalanced Flow / Thin Walls: Add secondary runners or auxiliary gates near the short-shot area. Consider increasing local wall thickness.
  • Improper Runner Sizing: Runners that are too small cause pressure loss; runners that are too large waste energy. Use smooth, radiused transitions to reduce flow resistance.
  • Poor Venting: Trapped air creates back-pressure. Utilize parting line venting, add vent grooves, or use vacuum venting systems to allow air to escape.

Comparison of a fully filled injection molded part versus a short shot defect.


Conclusie

Mastering injection molding requires a systematic approach to troubleshooting. By understanding the root causes of bubbles, sprue sticking, slow production cycles, and short shots, manufacturers can significantly reduce scrap rates and improve overall equipment effectiveness (OEE).

Are you still experiencing injection molding defects? Contact our engineering team today for a comprehensive mold flow analysis and process optimization consultation!

Over de auteur

Alex Yu

Alex Yu

Ideal Pro Manufacturing

Alex is medeoprichter van Ideal Pro, maar wanneer hij niet toezicht houdt op belangrijke projecten of leiding geeft aan het technische team, is hij waarschijnlijk bezig met een lange fietstocht, op zoek naar de beste koffie van de stad, of bezig met het plannen van zijn volgende reisavontuur. Met meer dan 20 jaar ervaring op het gebied van internationale handel en projectmanagement heeft hij het allemaal al meegemaakt: strakke deadlines, lastige technische vraagstukken en alles daartussenin. Hij is ervan overtuigd dat uitstekend werk voortkomt uit een uitgeruste geest en een goede kop koffie, en hij brengt diezelfde nieuwsgierigheid en oog voor detail mee in elk project dat hij aanneemt. Als hij niet op kantoor is, bevindt hij zich meestal ergens in de buitenlucht, waar hij nieuwe plekken verkent en verhalen verzamelt om te delen.