Injection Molding Shrinkage: The Impact of Temperature and Speed

Shrinkage (sink marks and voids) is one of the most common defects in injection molding. It occurs when the molten plastic cools and shrinks, leaving a void because the gate has sealed off before enough material could compensate for the contraction.

While many technicians know the basics, there are counter-intuitive factors that often make the problem worse. This article explores how Température du moule, Température de fusion, et Injection Speed[^1] specifically influence shrinkage.


Mold Temperature: Why "Too Cold" Can Be Bad

A common misconception is that lowering the mold temperature always helps reduce shrinkage. While high mold temperatures do prolong cooling time and can lead to shrinkage, mold temperature that is too low is equally detrimental.

The Mechanism of Failure

When the mold temperature is too low, the melt cools too rapidly.

  • Blocked Channels: In thick sections far from the gate, the outer skin freezes quickly. This seals off the channel, preventing molten plastic from the gate from reaching the core to compensate for shrinkage.
  • Concentrated Shrinkage: Low mold temperatures do not favor uniform overall shrinkage. Instead, they increase "concentrated shrinkage," making sink marks more severe and obvious.

Diagram showing how low mold temperature causes premature freezing and prevents shrinkage compensation.

> Conseil de pro : When troubleshooting difficult shrinkage issues, check your mold temperature. For materials like Polycarbonate (PC)[^2], which are prone to voids, increasing the mold temperature can significantly improve the issue, whereas low temperatures will seal the gate too early.


Melt Temperature: The Balance of Fluidity

Most operators know that high melt temperatures can cause shrinkage due to longer cooling times. The standard reaction is to lower the temperature by 10~20°C. However, setting the melt temperature too low (near the lower limit) is a critical error, especially for thick parts.

Why Low Melt Temperature Worsens Shrinkage

  • Premature Freezing: Similar to low mold temperature, if the melt is too cool, it condenses too fast.
  • Lack of Pressure Transmission: A sufficient temperature difference is needed from the shrinkage location back to the gate to allow for feeding. If the melt is too cold, the "feeding channel" freezes off before the part is packed out.
  • Material Sensitivity: This is very common with fast-condensing materials like PC.

Graph illustrating the relationship between melt temperature and viscosity in injection molding

Troubleshooting Step: Do not just look at the thermometer. Perform an air shot (purge) to visually inspect the melt quality and fluidity. If the melt looks stiff or rough, the temperature might be too low to solve the shrinkage problem.


Injection Speed: Slower Can Be Better

When shrinkage occurs, the instinct is to increase injection pressure and time. However, if your injection speed is too fast, it can actually hinder the solution.

The Benefits of Reducing Injection Speed

Slowing down the injection speed helps in two major ways:

  1. Thermal Gradient: It creates a larger temperature difference between the flow front and the gate. This promotes sequential solidification (freezing from far to near), allowing the gate to stay open longer for feeding.
  2. Pressure Application: It allows higher pressure to reach the shrinkage areas far from the gate.

Multi-stage injection profile showing slow speed and high pressure for packing phase to reduce shrinkage.Multi-stage injection profile showing slow speed and high pressure for packing phase to reduce shrinkage.

The Strategy: Slow Down to Speed Up Quality

By reducing the injection speed, the melt at the front is cooler and moves slower, reducing the risk of flash (burrs). This allows you to safely increase the pression de maintien et holding time, which are critical for eliminating shrinkage.

Recommended Profile:

  • Use a slow speed, high pressure, and long time profile for the final stage of injection (packing).
  • Try a "decelerating injection" profile (gradually slowing down while increasing pressure).

> Avertissement : Do not fill the cavity too slowly. If the fill time is excessive, the melt will freeze completely before the cavity is full, making compensation impossible.


Summary Table

ParamètresCommon MistakeOptimized Approach for Shrinkage
Mold TempSetting it too low to cool fast.Ensure it is not too low; maintain a temp that allows feeding channels to stay open.
Melt TempLowering it to the minimum limit.Keep it within the optimal range to ensure fluidity for packing.
vitesseInjecting as fast as possible.Reduce speed (especially in later stages) to allow for higher packing pressure.


[^1]: Learning about injection speed can help you adjust your process for better results and fewer defects. [^2]: Understanding the properties of PC can help you choose the right materials and settings for your projects.

À propos de l'auteur

Alex Yu

Alex Yu

Ideal Pro Manufacturing

Alex est le cofondateur d’Ideal Pro, mais lorsqu’il ne supervise pas des projets clés ou ne dirige pas l’équipe technique, vous le trouverez sans doute en train de faire une longue balade à vélo, à la recherche du meilleur café de la ville, ou en train de planifier sa prochaine aventure de voyage. Fort de plus de 20 ans d’expérience dans le commerce international et la gestion de projets, il a tout vu : délais serrés, problèmes techniques complexes et tout ce qui se trouve entre les deux. Il est convaincu qu’un travail de qualité naît d’un esprit bien reposé et d’une bonne tasse de café, et il apporte cette même curiosité et ce même souci du détail à chaque projet qu’il entreprend. Lorsqu’il n’est pas au bureau, il se trouve généralement en plein air, à explorer de nouveaux endroits et à glaner des anecdotes à partager.

Articles récents du blog

Impression 3D haute résolution : ce que la précision de 25 microns ne vous dit pas sur votre pièce
 

Impression 3D haute résolution : ce que la précision de 25 microns ne vous dit pas sur votre pièce

La hauteur de couche, la taille minimale des détails et la tolérance dimensionnelle constituent trois limites indépendantes. Il convient de prendre en compte les calculs relatifs aux chiffres publiés pour chaque processus, le niveau de finition requis et l'échantillon qui en apporte la preuve avant de valider la pièce.

avatar de blog Alex Yu
18 novembre 2026
Déformation lors de l'impression 3D : contraction, contrainte et le moment où les paramètres cessent d'être efficaces
 

Déformation lors de l'impression 3D : contraction, contrainte et le moment où les paramètres cessent d'être efficaces

Le gauchissement est une contrainte qui s'oppose à la contraction, et cette contraction provient du polymère plutôt que de votre logiciel de découpage. Le calcul des déplacements sur une portée réelle, qui ne tient compte que des contraintes d'ajout, permet d'usiner cette face à moindre coût qu'une quatrième tentative.

avatar de blog Alex Yu
18 novembre 2026
Pièces transparentes et translucides : la clarté relève d'une discipline de fabrication, et non d'un choix de matériau
 

Pièces transparentes et translucides : la clarté relève d'une discipline de fabrication, et non d'un choix de matériau

Les pièces transparentes présentent des défauts dus à l'humidité, à la contamination, à l'outillage à froid et à la présence d'air emprisonné. Veuillez préciser les valeurs de voile et de transmittance conformément à la norme ASTM D1003 au lieu d'indiquer " doit être transparent " sur le dessin.

avatar de blog Alex Yu
17 novembre 2026
Moulage par injection assisté par gaz : nervures creuses, gain de poids et les vides qui trahissent le procédé
 

Moulage par injection assisté par gaz : nervures creuses, gain de poids et les vides qui trahissent le procédé

Le gaz remplace la pression de compactage, et non la pression d'injection. Ce que le moulage assisté par gaz permet réellement de gagner en termes de masse, de tonnage de serrage et de temps de cycle, ainsi que de réduire les défauts liés au dégazage qui apparaissent ultérieurement sur la chaîne de peinture.

avatar de blog Alex Yu
17 novembre 2026